Vacuum Gas-Nitriding Furnace Produces Precision Nitrided Parts

Vacuum Gas-Nitriding Furnace Produces Precision Nitrided Parts

Donald Jordan, Solar Atmospheres; Heat Treating Progress, September 2009 - Currently, nitriding is carried out predominantly in pit type vertical furnaces with metal alloy retorts to hold the work load during the nitriding cycle. The large...

Learn more about Vacuum Gas-Nitriding Furnace Produces Precision Nitrided Parts

Low Torr-Range Vacuum Nitriding of 4140 Steel

Low Torr-Range Vacuum Nitriding of 4140 Steel

Don Jordan, Harry Antes, Virginia Osterman and Trevor Jones, Solar Atmospheres; Heat Treating Progress, March 2008 - Although the nitrided surfaces from atmospheric pressure nitriding and low-torr nitriding are similar, there are some...

Learn more about Low Torr-Range Vacuum Nitriding of 4140 Steel

The Advantages of Ion Nitriding Gears

The Advantages of Ion Nitriding Gears

Robert Lamont, Jr., Atch-Mont Gear Inc & A. Bruce Craven, Solar Atmospheres; Gear Technology, November 1996 - Ion Nitriding gears has the potential to eliminate the need for expensive post-heat treatment operations. The advantages of ion...

Learn more about The Advantages of Ion Nitriding Gears

Ion Nitriding Principles and Applications

Ion Nitriding Principles and Applications

A. Bruce Craven, Solar Atmospheres; Industrial Heating, May 1989 - Ion nitriding is a case hardening process that has been in existence in Europe for many years.  In the U.S., no attempt was made to use this process in production until...

Learn more about Ion Nitriding Principles and Applications