Austempering at Conventional Sintering Temperatures
William R. Jones, Solar Atmospheres, Inc.
Kenneth H. Moyer, Magna-Tech P/M Labs,...
Learn more about Austempering at Conventional Sintering Temperatures
Vacuum Sintering-A Way to Improve Ductility and Toughness of Structural P/M Parts at the Right Price
Kenneth H. Moyer, Magna-Tech P/M Labs, William R. Jones, Vacuum Furnace Systems, Inc., Ronald D. Payne, Sinteris PM Corporation - Most parts fabricators do not understand the importance of a quality sinter to provide improved ductility...