Utilization of Vacuum Technology in the Processing of Refractory Metal, Titanium and their Alloys for Powder Applications
Virginia M. Osterman, Solar Atmospheres; Industrial Heating, May 2008
Increased usage of refractory metals, titanium and their alloys in the aerospace and electronics industries has led to the use of the hydride/dehydride (HDH)...