Note: Part sizes and weight can exceed the dimensions and capability given based on placement and configuration in the furnace. Please contact a Solar sales engineer to determine if your parts can be processed.

Static Cooling Vacuum Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-32
6" dia. X 10" high
3200°F/ 1760°C
25
HT-46
12" wide X 12" high X 35" deep
3600°F/ 1982°C
500
HT-52
24" wide X 30" high X 18" deep
1200°F/ 649ºC
1,000
HT-66
8" dia. 12" deep
2750°F/ 1510 °C
100
2 Bar Quench Vacuum Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-1
24" wide X 24" high X 36" deep
(all metal hot zone)
2400°F/ 1315°C
1500
HT-5
40" wide X 30" high X 50" deep
2800°F/ 1573°C
4000
HT-10
24" wide X 24" high X 36" deep
2800°F/ 1573°C
1500
HT-13
60" wide X 48" high X 120" deep
2650°F/ 1454°C
10,000
HT-14
48" wide X 40" high X 72" deep
2800°F/ 1573°C
6,000
HT-20
14" wide X 12" high
2400°F/ 1315°C
50
HT-23
24" wide X 24" high X 36" deep
2800°F/ 1573°C
1,500
HT-33
60" wide X 48 " high X 144" deep
2650°F/ 1454°C
15,000
HT-36
36" wide X 30" high X 48" deep
2400°F/ 1315°C
3,500
HT-48
14" wide X 12" high X 30" deep
2650°F/ 1454°C
750
HT-49
60" wide X 48" high X 288" deep
2400°F/ 1315°C
75,000
HT-68
60" wide X 48" high X 144" deep
2800°F/ 1573°C
50,000
HT-69
68" wide X 84" high X 74" deep
2100°F/ 1149°C
15,000
HT-70
48" wide X 39" high X 96" deep
2650°F/ 1454°C
6,000
HT-73 65” wide x 65” high x 144” deep 2400°F/ 1315°C 50,000
HT-74 60” wide x 48” high x 288” deep 2400°F/ 1315°C 75,000
HT-78 60” wide x 48” high x 288” deep 2400°F/ 1315°C 75,000
HT-79 60” wide x 48” high x 432” deep 2400°F/ 1315°C 75,000
10 Bar Quench Vacuum Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-28
36" wide X 36" high X 50" deep
(6 bar quench)
2650°F/ 1454°C
3,500
HT-31
24" wide X 24" high X 36" deep
2650°F/ 1454°C
1,500
HT-28
40" wide X 36" high X 50" deep
2650°F/ 1454°C
3,500
HT-44
40" wide X 36" high X 50" deep
2650°F/ 1454°C
3,500
HT-50
24" wide X 24" high X 36" deep
2650°F/ 1454°C
1,500
HT-51
40" wide X 36" high X 50" deep
2650°F/ 1454°C
3,500
HT-58
48" wide X 40" high X 72" deep
2650°F/ 1454°C
10,000
HT-61
18" wide X 12" high X 30" deep
2650°F/ 1454°C
750
HT-62
18" wide X 12" high X 30" deep
2650°F/ 1454°C
750
10 Bar Vacuum Carburizing Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-61
18” wide x 12” high x 30” deep
2650ºF/ 1454ºC
750
HT-72
24” wide x 24” high x 72” deep
2400°F
1500
Ion Nitriding Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-11
12" dia. X 24" high
1200°F/ 649°C
500
HT-18
12" dia. X 24" high
1200°F/ 649°C
500
HT-19
30" dia. X 17 " high
1200°F/ 649°C
3,000
HT-4
30" dia. X 54" high
1200°F/ 649°C
3,000
Surface Treatment Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-65
7" dia. 12" high
3000°F/ 1650°C
100
HT-81
33" wide x 32" high x 47" deep
1400°F/ 760°C
2500
Air Tempering Furnaces
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-12
18" wide X 15" high X 19" deep
550°F/ 287°C
50
HT-21
24" wide X 24" high X 48" deep
1350°F/ 732°C
1,500
HT-24
19" wide X 18" high X 19" deep
1200°F/ 649°C
750
HT-25
19" wide X 18" high X 19" deep
1200°F/ 649°C
750
HT-27
15" wide X 14" high X 19" deep
450°F/ 232°C
100
HT-34
48" wide X 39" high X 54" deep
1400°F/ 760°C
5,000
HT-35
24" wide X 24" high X 48" deep
1100°F/ 593°C
500
HT-53
48" wide X 39" high X 60" deep
1400°F/ 760ºC
5,000
HT-54
24" wide X 24" high X 36" deep
1200°F/ 649ºC
1,500
HT-71
24" wide X 24" high X 36" deep
1200°F/ 649ºC
500
Cryogenic Treatment Freezers
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
DF-15
24" wide X 24" high X 48" deep
-300°F/ -184°C
2,000
DF-16
18" wide X 18" high X 18" deep
-120°F/ -85°C
1,000
DF-57
18" wide X 18" high X 18" deep
-120°F/ -85°C
1,000
DF-75
60" wide X 60" high X 60" deep
-300°F/ -184°C
2,000
Steam Treating / Tempering Furnace
Furnace #
Dimensions
Max Temperature
Max Load (lbs)
HT-2
22" dia. X 30" high
1100°F/ 593°C
1,000
 