To receive Solar Atmosphere’s newsletters, updates, events, fill out the form below.

Capabilities

Static Cooling Vacuum Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs) Location
HT-32
6" dia. X 10" high
3200°F/ 1760°C
25
Souderton, PA
HT-46
12" wide X 12" high X 35" deep
3600°F/ 1982°C
500
Souderton, PA
HT-66
8" dia. X 12" deep
2750°F/ 1510 °C
100
Souderton, PA

Back to Top

2 Bar Quench Vacuum Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs)
Location
HT-1
24" wide X 24" high X 36" deep
(all metal hot zone)
2400°F/ 1315°C
1500
Souderton, PA
HT-5
40" wide X 30" high X 50" deep
2800°F/ 1573°C
4000
Souderton, PA
HT-10
24" wide X 24" high X 36" deep
2800°F/ 1573°C
1500
Souderton, PA
HT-13
60" wide X 48" high X 120" deep
2650°F/ 1454°C
10,000
Souderton, PA
HT-14
48" wide X 40" high X 72" deep
2800°F/ 1573°C
6,000
Souderton, PA
HT-20
14" wide X 12" high
2400°F/ 1315°C
50
Souderton, PA
HT-23
24" wide X 24" high X 36" deep
2800°F/ 1573°C
1,500
Souderton, PA
HT-33
83" Dia. X 144" deep
2650°F/ 1454°C
15,000
Souderton, PA
HT-36
36" wide X 30" high X 48" deep
2400°F/ 1315°C
3,500
Souderton, PA
HT-48
14" wide X 12" high X 30" deep
2650°F/ 1454°C
750
Souderton, PA
HT-73
83” Dia. X  144” deep 2400°F/ 1315°C 50,000 Souderton, PA

Back to Top

10 Bar Quench Vacuum Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs)
Location
HT-28
36" wide X 36" high X 50" deep
(6 bar quench)
2650°F/ 1454°C
3,500
Souderton, PA
HT-31
24" wide X 24" high X 36" deep
2650°F/ 1454°C
1,500
Souderton, PA
HT-44
40" wide X 36" high X 50" deep
2650°F/ 1454°C
3,500
Souderton, PA
HT-58
48" wide X 40" high X 72" deep
2650°F/ 1454°C
10,000
Souderton, PA
HT-61
18" wide X 12" high X 30" deep
2650°F/ 1454°C
750
Souderton, PA

Back to Top

10 Bar Vacuum Carburizing Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs)
Location
HT-61
18” wide X 12” high x 30” deep
2650ºF/ 1454ºC
750
Souderton, PA
HT-72
24” wide x 24” high X 72” deep
2400°F
1500 Souderton, PA

Back to Top

Ion Nitriding Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs)
Location
HT-11
12" dia. X 24" high
1200°F/ 649°C
500
Souderton, PA
HT-18
12" dia. X 24" high
1200°F/ 649°C
500
Souderton, PA
HT-19
30" dia. X 17 " high
1200°F/ 649°C
3,000
Souderton, PA
HT-4
30" dia. X 54" high
1200°F/ 649°C
3,000
Souderton, PA

Back to Top

Surface Treatment Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs)
Location
HT-65
7" Dia. X 12" high
3000°F/ 1650°C
100
Souderton, PA
HT-81
33" wide X 32" high X 47" deep
1400°F/ 760°C
2500
Souderton, PA

Back to Top

Air Tempering Furnaces

Furnace #
Hot Zone Dimensions
Max Temperature
Max Load (lbs)
Location
HT-12
18" wide X 15" high X 19" deep
550°F/ 287°C
50
Souderton, PA
HT-21
24" wide X 24" high X 48" deep
1350°F/ 732°C
1,500
Souderton, PA
HT-24
19" wide X 18" high X 19" deep
1200°F/ 649°C
750
Souderton, PA
HT-25
19" wide X 18" high X 19" deep
1200°F/ 649°C
750
Souderton, PA
HT-27
15" wide X 14" high X 19" deep
450°F/ 232°C
100
Souderton, PA
HT-34
48" wide X 39" high X 54" deep
1400°F/ 760°C
5,000
Souderton, PA
HT-35
24" wide X 24" high X 48" deep
1100°F/ 593°C
500
Souderton, PA
HT-71
24" wide X 24" high X 36" deep
1200°F/ 649ºC
500
Souderton, PA

Back to Top

Cryogenic Treatment Freezers

Furnace #
Dimensions
Max Temperature
Max Load (lbs) Location
DF-15
24" wide X 24" high X 48" deep
-300°F/ -184°C
2,000
Souderton, PA
DF-16
18" wide X 18" high X 18" deep
-120°F/ -85°C
1,000
Souderton, PA
DF-94
52" wide X 52" high X 96" deep
-300°F/ -184°C
10,000
Souderton, PA

Back to Top