Capabilities

Static Cooling Vacuum Furnaces

Furnace #
Dimensions
Max Temperature
Max Load (lbs) Location
HT-52
24" wide X 30" high X 18" deep
1200°F/ 649ºC
1,000
Hermitage, PA

Back to Top

2 Bar Quench Vacuum Furnaces

Furnace #
Dimensions
Max Temperature
Max Load (lbs)
Location
HT-49
84" Dia. X 288" deep
2400°F/ 1315°C
75,000
Hermitage, PA
HT-68
84" Dia. X 144" deep
2800°F/ 1573°C
50,000
Hermitage, PA
HT-69
68" wide X 84" high X 74" deep
2100°F/ 1149°C
15,000
Hermitage, PA
HT-74
84" Dia. X 288” deep 2400°F/ 1315°C 75,000 Hermitage, PA
HT-78
84" Dia. X 288” deep 2400°F/ 1315°C 75,000 Hermitage, PA
HT-79
84" Dia. X 432” deep 2400°F/ 1315°C 150,000 Hermitage, PA

Back to Top

10 Bar Quench Vacuum Furnaces

Furnace #
Dimensions
Max Temperature
Max Load (lbs)
Location
HT-50
24" wide X 24" high X 36" deep
2650°F/ 1454°C
1,500
Hermitage, PA
HT-51
40" wide X 36" high X 50" deep
2650°F/ 1454°C
3,500
Hermitage, PA
HT-62
18" wide X 12" high X 30" deep
2650°F/ 1454°C
750
Hermitage, PA

Back to Top

Air Tempering Furnaces

Furnace #
Dimensions
Max Temperature
Max Load (lbs)
Location
HT-53
48" wide X 39" high X 60" deep
1400°F/ 760ºC
5,000
Hermitage, PA
HT-54
24" wide X 24" high X 36" deep
1200°F/ 649ºC
1,500
Hermitage, PA

Back to Top

Cryogenic Treatment Freezers

Furnace #
Dimensions
Max Temperature
Max Load (lbs) Location
DF-57
18" wide X 18" high X 18" deep
-120°F/ -85°C
1,000
Hermitage, PA
DF-75
60" wide X 60" high X 60" deep
-300°F/ -184°C
2,000
Hermitage, PA