Melting Points Booklet Technical Articles
A 20 page booklet, "The Critical Melting Points of Metals and Alloys" was published in January of 1998 and has been in demand by hundreds of companies. The booklet lists melting points for the following materials: stainless steel, corrosion- resistant steel castings, heat-resistant alloy castings, aluminum and aluminum casting alloys, copper and copper casting alloys, magnesium alloys/casting alloys, magnesium alloys/wrought alloys, nickel alloys, tin alloys, zinc alloys, precious metal alloys, Ni-Cr-Mo-Cu alloys, electrical resistance alloys, titanium alloys and eutectics. Tables for the Vapor Pressure of Elements in Torr and Equivalence for Pressure/Vacuum Measurements are also listed. Individual copies upon request, multiple copies for a small fee. To order call 800-347-3236 or email info@solaratm.com.
|